Electronics Forum | Tue May 06 11:56:56 EDT 2008 | joeherz
We have a board that uses 0402x4 RNET packages that we are having a difficult time getting to solder consistently. Paste deposition is fine (using AIM WS353) and profile is dead-nuts. I'm starting to wonder if this is something that we're just goin
Electronics Forum | Tue Dec 19 10:08:10 EST 2006 | George
Grant, Why don't you try a water-base flux which is No-clean, VOC-free also? I have tried the 270WR flux from AIM with good results even on lead-free process. My $0.02, George
Electronics Forum | Thu May 13 20:40:25 EDT 2021 | winston_one
Yes, we can't use pure Pb PROCESS. And as I say we will not use it anyway, as we have lead-free BGA's, LGAs, component with Solder Charged Terminations... It's became almost normal practice to solder it with leaded solder pastes. In this case peak re
Electronics Forum | Tue Aug 22 10:06:53 EDT 2000 | George English
Has there been a definite date for the total move over to lead free? Will it be 2004 or 2008. Also is there a direct replacement for leaded solder, I have read various articles on numerous alloys suggested for the switch, such as bismuth, tin, copper
Electronics Forum | Mon Dec 18 23:24:50 EST 2006 | grantp
Hi, Yes, I would hate to resort to cleaning, but the product must be clean. We have been using palettes to keep most of the flux off the PCB, but there is still residue around the connectors. Does anyone suggest a good no clean flux to use with le
Electronics Forum | Tue Sep 17 15:40:59 EDT 2013 | 18424
Good day all, I wanted to get a quick poll from the folks running SAC305 in their selective soldering equipment. How are final results? How repeatable is the process, any machine related failures? pumps? nozzles? etc... I am just looking to get a
Electronics Forum | Tue Sep 17 15:47:04 EDT 2013 | 18424
Good day all, I wanted to get a quick poll from the folks running SAC305 in their selective soldering equipment. How are final results? How repeatable is the process, any machine related failures? pumps? nozzles? etc... I am just looking to get a
Electronics Forum | Fri Dec 15 18:36:46 EST 2006 | Grant
Hi, I have noticed we are getting residue on our wave pcb's and it's worse with lead free, since we changed to the flux we are using. We are currently using Avantec VOC Free flux model Ecofree 303. It looks like it's made in Malaysia. Does anyone h
Electronics Forum | Thu May 01 15:11:37 EDT 2008 | dphilbrick
CK So as I see it batch B represents a leaded process with leaded components and D is a leaded process with lead free components. Batch Components Paste B SnPb Sn62 D Lead-free Sn62 If so it is BETTER to run a lead free BGA with Sn
Electronics Forum | Thu Jul 15 12:09:10 EDT 2010 | wrongway
if the BGA has leaded balls use leaded paste if the BGA has lead free balls use lead free paste and set your oven profile to match the paste